Phosphoric acid-impregnated clay bricks are alkali-resistant coke stones and binders that are first granulated and powdered, mixed at a certain ratio, compressed and molded, fired at high temperature, impregnated with phosphoric acid solution, and then calcined again Stronger products.
Items | Behaviors |
Al2O3, % ≥ | 41-45 |
P2O5, % ≥ | 7 |
Fe2O3 % ≤ | 1.4 |
0.2Mpa Load softening temperature≥ | 1450 |
Reheating Linear Change % | 0~-0.2 |
Apparent Porosity,% ≤ | 14 |
Cold Crushing Strength, Mpa ≥ | 55 |
Alkali resistance (strength drop rate) | 15 |
If you are interested in our products, please leave your contact information and products, we will reply you in time.